Does ASME Sect 8 Tell you to have a smooth Ground flush finish on the inside Weld of the Nozzle for a pressure Vessel? or is it something that I need to specifically tell my vendor, if I require it ?.

If ASME tells you, can I please have the Section number.

Thank You
 
You need to tell your vendor and preferably on your drawing.
 
Depends of dimensions, materials and service:

1) If the pressure vessel is stainless steel and hygienic design, obviously inside surface shall be smooth and polished, ….and more good engineering practice other than ASME VIII

2) UHT-84 WELD FINISH
The requirements of UW-35(a) and UW-51(b) shall be
met except that for SA-517 material the maximum weld
reinforcement shall not exceed 10% of the plate thickness
or 1/8 in. (3.0 mm), whichever is less. The edge of the weld
deposits shall merge smoothly into the base metal without
undercuts or abrupt transitions; this requirement
shall apply to fillet and groove welds as well as to butt
welds.

Regards
r6155
 
It is not required for a nozzle that has an inside projection. If you want it done, specify it. BTW it is Section VIII.

Regards,

Mike