Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME SEC VIII Div 1 Appendix 31

Status
Not open for further replies.

bmoorthy

Mechanical
May 29, 2003
457
Hello

Appendix clause 31-4 of ASME SEC VIII Div 1 specifies that welding shall be limited to SAW and SMAW whereas the table 31.2 gives composition for GTAW and GMAW weld metal.

Is this an inconsistency? or is there some other meaning to this?
 
Replies continue below

Recommended for you

Re-read 31-4(a) says SAW or SMAW for 3Cr-1Mo-1/4V-Ti-b material ONLY.
 
Thankyou. I realised i was refering 1998 addenda. On checking the 2001 addenda the inconsistency(it was an inconsistency after all) was found to have been rectified.

 