Dish to shell welding has been completed RT results pass, but while visual inspection, one of my friend saw that there no taper has been done on that joint there 4 mm difference in dish head thickness and shell thickness, should we need to reject that joint or need to accept, give me the reference.
Best rgds
I need your answer,
Dish to shell welding has been completed RT results pass, but while visual inspection, one of my friend saw that there no taper has been done on that joint there 4 mm difference in dish head thickness and shell thickness, should we need to reject that joint or need to accept, give me the reference.