Carbon, max 0.30; Manganese 0.60¨C1.35; Phosphorus,max
0.035; Sulfur, max 0.040; Silicon 0.15¨C0.30; Nickel 0.40 max; Chromium 0.30 max; Molybdenum 0.12 max; Copper 0.40 max; Columbium 0.02 max; Vanadium 0.05 max.

Tensile strength, 70¨C95 ksi; Yield strength, min, 36 ksi.
 