Hi guys,
New to this forum. I Have a question about pipe dimensions: Can I use pipe with dimensions that are not listed in SA-312 table X1.1? For example, in SA-312, NPS 2 has OD 2.375" (60.33mm), wall thickness of 0.218"(5.54mm), can I used 68mm*12mm (OD x wall thickness) as ASME SA-312 material if the manufacture can make this pipe? Couldn't find any specification guiding this.
Thank you very much for sharing your advice!
New to this forum. I Have a question about pipe dimensions: Can I use pipe with dimensions that are not listed in SA-312 table X1.1? For example, in SA-312, NPS 2 has OD 2.375" (60.33mm), wall thickness of 0.218"(5.54mm), can I used 68mm*12mm (OD x wall thickness) as ASME SA-312 material if the manufacture can make this pipe? Couldn't find any specification guiding this.
Thank you very much for sharing your advice!