Mar 27, 2018 #1 sshh Civil/Environmental Joined Mar 27, 2018 Messages 5 Location US Hi, Which section of asme code specifies the minimum elongation of 40 % for sa 240 304 L? Thanks http://files.engineering.com/getfile.aspx?folder=8e28773f-2fcc-4adf-a3af-3a415c49c504&file=properties.docx
Mar 27, 2018 #2 EdStainless Materials Joined May 20, 2004 Messages 16,366 Location Waukesha WI USA Sec II part D with the other material specifications. Why do you doubt it? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Sec II part D with the other material specifications. Why do you doubt it? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Mar 27, 2018 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US ASME Section II, Part A material specification, Table 2 of SA 240. Upvote 0 Downvote
Mar 27, 2018 #4 EdStainless Materials Joined May 20, 2004 Messages 16,366 Location Waukesha WI USA Sorry, thanks Metengr. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Mar 27, 2018 Thread starter #5 sshh Civil/Environmental Joined Mar 27, 2018 Messages 5 Location US Thanks metengr. Found it. Upvote 0 Downvote