Feb 8, 2016 #1 OzzieT Materials Joined Aug 25, 2015 Messages 1 Location US My question is as follows: If a welder is qualified to weld on a pipe >2.5 NPS does this qualify him/her to weld a fillet weld on a pipe <2.5 NPS?
My question is as follows: If a welder is qualified to weld on a pipe >2.5 NPS does this qualify him/her to weld a fillet weld on a pipe <2.5 NPS?
Feb 8, 2016 #2 DVWE Petroleum Joined Apr 5, 2007 Messages 2,373 Location US Did the welder qualify on a groove weld, or fillet weld? Upvote 0 Downvote
Feb 8, 2016 #3 SectionIX Petroleum Joined Sep 19, 2011 Messages 283 Location US No, if qualified by a fillet in accordance with ASME IX, Table QW-452.4; Yes if qualified by groove weld per ASME IX Table QW-452.6. Upvote 0 Downvote
No, if qualified by a fillet in accordance with ASME IX, Table QW-452.4; Yes if qualified by groove weld per ASME IX Table QW-452.6.