ASME Annex 3.D has some equations that can be used to create True Stress X True Strain curves for several classes of materials.
No problem putting them on an Excel.
I'll start my doubt showing a piece of an example that I have generated with these equations (just what I believe to be the first point ---> yield stress), for SA-285C (Su=380 MPa; Sy=205 MPa; E=200000 MPa):
st [MPa] ets e_elástico ETS_PLÁSTICO
205 0.003143883 0.001014851 0.002129031
The first collumn is the stress, ets= total true strain; e_elastico=elastic strain and ETS_PLÁSTICO=plastic strain.
My doubt is: shouldn't the value of plastic strain be zero for the yield stress??
Other question: I've seen one ASME Examples book where it is found the proportional limit using these equations. And plastic strain was set to zero for the proportional limit. Ok! But the example doesn't explain how to obtain the proportional limit from the ASME Annex 3.D MPC equations.
If necessary, I can send my Excel spreadsheet.
Thanks a lot if someone can clarify me.
_______________________________
Hervandil Sant'Anna
Petrobras
ASME Annex 3.D has some equations that can be used to create True Stress X True Strain curves for several classes of materials.
No problem putting them on an Excel.
I'll start my doubt showing a piece of an example that I have generated with these equations (just what I believe to be the first point ---> yield stress), for SA-285C (Su=380 MPa; Sy=205 MPa; E=200000 MPa):
st [MPa] ets e_elástico ETS_PLÁSTICO
205 0.003143883 0.001014851 0.002129031
The first collumn is the stress, ets= total true strain; e_elastico=elastic strain and ETS_PLÁSTICO=plastic strain.
My doubt is: shouldn't the value of plastic strain be zero for the yield stress??
Other question: I've seen one ASME Examples book where it is found the proportional limit using these equations. And plastic strain was set to zero for the proportional limit. Ok! But the example doesn't explain how to obtain the proportional limit from the ASME Annex 3.D MPC equations.
If necessary, I can send my Excel spreadsheet.
Thanks a lot if someone can clarify me.