The criteria for establishing allowable stress table 1-100 of the ASME II Part.D also apply to seamless tubes?
Greetings.
 
Replies continue below

Recommended for you

tiagols, giving it a quick scan, I don't see any references to product form.

Regards,

Mike
 
Tiaglos,
Answer to your question is "yes".

Seamless tubes fall under first row of Table 1-100 while welded tubes fall under second row of Table 1-100.
For welded pipes or tubes, allowable stresses are lowered by 15% as those seamless.

Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
 
My scan was a little TOO quick it seems, agree w/ Fizza453. Apologies:)
 