cmsvessel

Mechanical
Nov 3, 2005
34
Could somebody indicate what we should do when we design, fabricate and inspect pressure vessels using ASME code but need PED for Europe country? Take pressure vessel made of SA516-70 as an exsample?
 
Replies continue below

Recommended for you

Be aware of the PED Hydrotest requirement of 1.43 x Design Pressure.
Sometimes this equates to a higher pressure than specified in UG-99 and additional checks are required to ensure the stresses during testing are below 90% Yield.

Also be careful with carbon steels. PED requires the Carbon Content to be less than 0.25% but some ASME materials (eg SA105) allows up to 0.35%
 