Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME BPVC VIII Div 2, ANNEX 3D.3, Proportional Limit, Stress Strain Curve

Status
Not open for further replies.

Doodler3D

Mechanical
Joined
Jan 20, 2020
Messages
188
Location
US
Hi,

I am performing an elastic-plastic simulation on a vessel. I've correctly generated the elastic plastic stress strain curve but I'm lost on the calculation of the proportional limit. I read the comments by TGS4 on the parent topic, but I'm still confused with the iterative procedure for the proportional limit? There's the arbitrary true plastic strain to be taken as 10^-6. Is it simply based off true strain(total) = True Elastic strain. I feel that I am overthinking the process after being muddled up in the definitions.

File attached for reference.

Thank you.
 
 https://files.engineering.com/getfile.aspx?folder=32e4cef7-1782-41e0-ae95-e0706bd75fb2&file=ASME_VIII_DIV_2+ANNEX_3D.3+Stress-Strain_Relationships.xlsx
Actually - the ASME Code Committee has clarified that the plastic strain at the proportional limit is the value of εp from Table 3-D.1.

Calculate the plastic strain (γ12) and determine the stress at which this value equals approximately εp.
 
By chance, I've been mulling over this for the last few weeks as well.
Perhaps in the next code update, the committee will improve the definition of εp.

I find it remarkable that when a stress equal to yield is exerted onto the spreadsheet, the plastic strain equals near enough exactly 0.2%, in line with ASME II Part D.
 
Thank you TGS4. I was indeed overthinking the simple.

Picture1_whaet5.png
 
I believe that the Code item improving the definition of the proportional limit with ε p was passed and it should be published in the 2021 Edition.
 
Status