Can anybody help me to find the ASME standard;
ASME B46.1 - 1995 (Revision of ANSI/ASME B46.1-1985) Surface Texture (Surface Roughness, Waviness, and Lay) for a scientific search?.....
 
Replies continue below

Recommended for you

On a related note, does anyone out there know of a roughness standard for polished surfaces? Does one just specify what grit to use for the final pass? For example, a polished brass bell may have a satin finish, mirror finish, or something in between. Is there a standard I can specify?

Thanks in advance,

Mike
 