JAYDEE23
Materials
- Jun 16, 2009
- 146
Can you please inform me as to how I go about determining allowable stress values @ temperature for ASTM material A707 L3CL3?
I will be using this material, as specified by my customer, to make a section of, what is essentially straight pipe for a B31.3 application.
I understand section 323.1.2 Unlisted Materials of B31.3 and Appendix 5 of section 2.
I just do not understand where to get yield or tensile values at temperature for ASTM material.
Any help is much appreciated.
I will be using this material, as specified by my customer, to make a section of, what is essentially straight pipe for a B31.3 application.
I understand section 323.1.2 Unlisted Materials of B31.3 and Appendix 5 of section 2.
I just do not understand where to get yield or tensile values at temperature for ASTM material.
Any help is much appreciated.