Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME B31.3 Process Piping Distortion (Dent) tolerance

Status
Not open for further replies.

kab6081

Mechanical
Dec 4, 2009
2
I am looking in ASME B31.3 for the distortion (dent) tolerance on process piping and have been unsuccessful. Please help in locating the section(s) which give the tolerance. Thank you.
 
Replies continue below

Recommended for you

I have not found any definition in B31.3, but in the gas code dents are defined in B31.8 Section 841.243 as follows,
(c) All dents that affect the curvature of the pipe at the longitudinal weld or any circumferential weld shall
be removed. All dents that exceed a maximum depth of
1?4 in. in pipe NPS 12 and smaller or 2% of the nominal
pipe diameter in all pipe greater than NPS 12 shall not
be permitted in pipelines or mains intended to operate
at hoop stress levels of 40% or more of the specified
minimum yield strength. When dents are removed, the
damaged portion of the pipe shall be cut out as a cylinder.
Insert patching and pounding out of the dents is
prohibited.

**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 
Thank you for the help and quick response.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor