Hi everybody,
With ASME B31.3 as construction code and ASME IX as qualification code.
Could I use PQR with PWHT with a WPS without PWHT ?
The thickness range in the WPS don't require PWHT according to ASME B31.3.
NB: The other parameters in the PQR and WPS comply with ASME IX.
Thanks and excuse me for my bad english.
With ASME B31.3 as construction code and ASME IX as qualification code.
Could I use PQR with PWHT with a WPS without PWHT ?
The thickness range in the WPS don't require PWHT according to ASME B31.3.
NB: The other parameters in the PQR and WPS comply with ASME IX.