Looking for some help on a material use issue.
In B31.1 Table 126.1:
A182 is listed as acceptable to use under Forgings
A182 is not listed under fittings
I have a Piping Book that states that A182 is not acceptable for fittings per B31.1
This has confused me a bit.
To me, it appears that A182 Forged Fitting are ok to use per B31.1
Am I correct in this??
(The same situation applies to A105 for Carbon Steel.....book says no good for Fittings...but B31.1. says ok for Forgings)
Thanks,
Mike
In B31.1 Table 126.1:
A182 is listed as acceptable to use under Forgings
A182 is not listed under fittings
I have a Piping Book that states that A182 is not acceptable for fittings per B31.1
This has confused me a bit.
To me, it appears that A182 Forged Fitting are ok to use per B31.1
Am I correct in this??
(The same situation applies to A105 for Carbon Steel.....book says no good for Fittings...but B31.1. says ok for Forgings)
Thanks,
Mike