Hello forum,
I apologies for posting this topic once again, since we were not able conclude by that time.
A) This is with reference to ASME B16.5 para 5.4.3 & ASME B31.3 Appendix F para F308.4. Is it prohibited to use of spiral wound gasket for class 150 slip on flanged joint?
B) Is it prohibited to use gaskets other than ASME B16.5 Non-mand appdx B, Table B-1, group no. I gaskets for class 150 slip on flanged joint?
I heard answers stating that these are only recommendation and hence not mandatory. But if it is recommendations and we dont want to follow them, we should have some sort of backup?
Please share your view.
GD_P
I apologies for posting this topic once again, since we were not able conclude by that time.
A) This is with reference to ASME B16.5 para 5.4.3 & ASME B31.3 Appendix F para F308.4. Is it prohibited to use of spiral wound gasket for class 150 slip on flanged joint?
B) Is it prohibited to use gaskets other than ASME B16.5 Non-mand appdx B, Table B-1, group no. I gaskets for class 150 slip on flanged joint?
I heard answers stating that these are only recommendation and hence not mandatory. But if it is recommendations and we dont want to follow them, we should have some sort of backup?
Please share your view.
GD_P