Hello,
we buy blind flanges according to B16.5, EN1092-1, etc. We make thermowells out of these flanges, and e.g. with 2500lbs full penetrant welded flanges, we get quite some distortion in the bolt holes.
For larger orders, we subcontract thermowells and we have one supplier that offers thermowells with perfect round holes. They are able to do so, because they drill the holes after welding.
Is this something we are allowed to do acc. to the b16.5 standard?
=>
Buy flanges according to B16.5 but without bolt holes. I checked with our supplier, and they will not be B16.5 marked obviously. Are we allowed to mark these B16.5 if we machine the holes after welding? Holes will be acc to the b16.5 standard.
I am curious about what is allowed and what not. If we stamp B16.5, do we need to be inspected by asme of some sort?
Thanks for your ideas.
Sam
we buy blind flanges according to B16.5, EN1092-1, etc. We make thermowells out of these flanges, and e.g. with 2500lbs full penetrant welded flanges, we get quite some distortion in the bolt holes.
For larger orders, we subcontract thermowells and we have one supplier that offers thermowells with perfect round holes. They are able to do so, because they drill the holes after welding.
Is this something we are allowed to do acc. to the b16.5 standard?
=>
Buy flanges according to B16.5 but without bolt holes. I checked with our supplier, and they will not be B16.5 marked obviously. Are we allowed to mark these B16.5 if we machine the holes after welding? Holes will be acc to the b16.5 standard.
I am curious about what is allowed and what not. If we stamp B16.5, do we need to be inspected by asme of some sort?
Thanks for your ideas.
Sam