Hi all,
I have problem in reviewing QC document for Pressure reducing desuperheating valve (PRDS)
material: A216 WCC
rating : ASME 600#
Plug and seat ring material: 410 SS (ANSI 410)
my question: i asked for NDE liquid penetrant (PT) test for hard facing area for plug and seat ring material.
The contractor replied:
1. NDE (PT) test is not required since the material is 410 SS, if the material is 316 SS (A276-316) then it is required.
2. the contractor said according to the ASME 16.34 the valves required for NDE are only for special class valve, otherwise not required for standard class valve.
What i want to know:
1. is the contractor explanation acceptable, according to the ASME 16.34. But the our agreed inspection plan covers NDE (PT).
2. what are the special class valves?
thanks.
I have problem in reviewing QC document for Pressure reducing desuperheating valve (PRDS)
material: A216 WCC
rating : ASME 600#
Plug and seat ring material: 410 SS (ANSI 410)
my question: i asked for NDE liquid penetrant (PT) test for hard facing area for plug and seat ring material.
The contractor replied:
1. NDE (PT) test is not required since the material is 410 SS, if the material is 316 SS (A276-316) then it is required.
2. the contractor said according to the ASME 16.34 the valves required for NDE are only for special class valve, otherwise not required for standard class valve.
What i want to know:
1. is the contractor explanation acceptable, according to the ASME 16.34. But the our agreed inspection plan covers NDE (PT).
2. what are the special class valves?
thanks.