ASME B16.20 covers SS Type 316 Ring Gaskets and indicates the hardness requirement as 160 HB max. Could the same requirement be specified for SS Type 316L Ring Gaskets
also ?
 
Replies continue below

Recommended for you

I don believe because the AISI 316 L It is low carbon.

Is THIS Right?.

Tecnico 1948
 