If I use an A320 B8 bolt in an ASME 8 vessel the max temperature it can see is only 100F, If I use an A193 B8 bolt it can see 1500F. Why is this as both bolts are basically 304 stainless steel, with identical UNS number and mechanical properties?
 
Replies continue below

Recommended for you

It's a matter of reference specifications: A320 is for low temperature service, A193 for high temperature service.
I agree that the two are quite similar, especially for austenitic steels, but the fabricator has to choose one and to fulfil it.