Can anybody talk to me if the old ASME 1204-10 steel have copper in its chemical composition?

Thank you in advance.

Mario Valenti
Argentina
 
Replies continue below

Recommended for you

MY books (3) list AISI 1024 as a carburizing steel and the analysis shows no Cu, not even a tramp limit.

You may have to get the ASME or ASTM specification to see what are the limits of Cu are. You also might check with your supplier about a couple of Material Test Reports of this material.
 