[ASK] Standard Provides Mechanical Properties for Alloy Steel 41XX 1

Status
Not open for further replies.

Rizkyffq

Mechanical
Joined
Jun 5, 2017
Messages
53
Location
ID
Hello sirs,
I am trying to create material spec for alloy steel 41XX.
I already got requirement for chemical composition in ASTM A29.
But the problem i still not get the standard that provides all alloy steel 41XX for mechanical properties.
what i got is only for 4130 and 4140, maybe someone that having knowledge about standard may give me an advise to choose what standard that provides value of mechanical properties requirement for alloy steel 41XX ?

Hopefully someone may help me, thanks in advance sirs
 
I'm not aware of any standard that includes properties for all 41XX steels. In the oil & gas industry, 4130 and 4140 are both very commonly used, but other 41XX alloys are not.
 
Thanks guy for the feedback
 