Apr 20, 2010 #1 Chacuncha Petroleum Joined Feb 11, 2009 Messages 8 Location GB We have an oilfield production of Oil-gas-water and we intend using the gas as boiler feed gas. Does anyone know if Arsenic is corrosive to steel in boiler gas firing and service? thank you