Anyone know what material this is? ARP just describes it as a high alloy martensitic q&t steel.
 
Replies continue below

Recommended for you

Based on the description, it is likely 1Cr-0.5Mo-0.25V (SAE AMS6304 conventional melting, 6305 VAR). The hardness range of 44-47 HRC is equivalent to UTS of 1400-1500 MPa, which is higher than that typically used for 8740.
 