Anyone know of a good link to the machinability of armor plate? Or anything that might get me close? At wits' end ~ I'll be guessing here soon.

 
Replies continue below

Recommended for you

Did you try this?


Title : Tool Bits and Drills for Machining Armor Plate,

Corporate Author : WATERTOWN ARSENAL MA

Personal Author(s) : Crawford,D. J.

Descriptors : *Drills, Machine tools, Drilling, Armor plate, Tool steel