Hi guys. Does anybody know if the Group Numbers in B16.5 are equivalent to Section IX P-numbers? I don't have a copy of Section IX. Thanks!
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
If they're not the same, how then does a guy ensure he is matching up equivalent metallurgies when welding or when assembling a piping design specification for a particular fluid service? Do you have to go back to the base ASTM specs and look at all the compositions and calculate the carbon equivalents, etc.?