Are alloy C276 pressed end caps from plate ASTM B366 permitted in PED vessels? There is an EAM for flat products according to ASTM B366, but does this cover pressed end caps? Or is it up to my inspector?
 
Replies continue below

Recommended for you

There is no subscription whatsoever for what parts you use in PED, just the strenght calculations have to be right.
 