Nov 22, 2023 #1 Oluwakay Mechanical Joined Sep 15, 2022 Messages 83 Location PL Hello Everyone, I want to ask, what is the easiest way to model and tensile a single yarn in abaqus? Thank you!
Hello Everyone, I want to ask, what is the easiest way to model and tensile a single yarn in abaqus? Thank you!
Nov 22, 2023 #2 FEA way Mechanical Joined Nov 13, 2018 Messages 5,200 Location PL It depends on its size and shape - if a reasonably dense solid mesh can be applied to it or if 1D elements have to be used. Upvote 0 Downvote
It depends on its size and shape - if a reasonably dense solid mesh can be applied to it or if 1D elements have to be used.
Nov 22, 2023 Thread starter #3 Oluwakay Mechanical Joined Sep 15, 2022 Messages 83 Location PL Can you suggest how both options could be explored on abaqus? I can assume the cross-section of the yarn is circular. Could it be modelled as 3D long pipe with a circular cross-section? Upvote 0 Downvote
Can you suggest how both options could be explored on abaqus? I can assume the cross-section of the yarn is circular. Could it be modelled as 3D long pipe with a circular cross-section?
Nov 24, 2023 1 #4 FEA way Mechanical Joined Nov 13, 2018 Messages 5,200 Location PL Beam elements should be sufficient so model this as a wire and assign a beam section with a circular profile. Upvote 0 Downvote
Beam elements should be sufficient so model this as a wire and assign a beam section with a circular profile.
Nov 27, 2023 Thread starter #5 Oluwakay Mechanical Joined Sep 15, 2022 Messages 83 Location PL Thank you so much! Upvote 0 Downvote