We have a stripper tank coated with Epoxy Resin ( 125 micorn DFT)on inner surface of it.
The tank handles Oxidized Neutralized Caustic Water, however the pH fluctuates dangerously and ranges between 4 to 11.The Service temp. is 50 deg. C
We are encountering frequent failire of tank wall and wall thinning has also taken place. Design Wall Thk: 5 mm
We have decided to replace the Epoxy Resin coating (125 mic) with a Epoxy Phenolic coating (150 mic DFT).
What is the difference between thse 2 coatings? Is Epoxy Phenolic Coating better than Epoxy Resin Coating for the given application?
Thanks.......
The tank handles Oxidized Neutralized Caustic Water, however the pH fluctuates dangerously and ranges between 4 to 11.The Service temp. is 50 deg. C
We are encountering frequent failire of tank wall and wall thinning has also taken place. Design Wall Thk: 5 mm
We have decided to replace the Epoxy Resin coating (125 mic) with a Epoxy Phenolic coating (150 mic DFT).
What is the difference between thse 2 coatings? Is Epoxy Phenolic Coating better than Epoxy Resin Coating for the given application?
Thanks.......