Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API650 Tank annular bottom plate and bottom plate

Status
Not open for further replies.

magmath76

Mechanical
Apr 27, 2011
20
Hi All,

If the tank bottom plate is 6mm and the annular bottom plate required also 6mm (as per table 5.1). In this case is it ok not to have the separate annular plate instead just extend the bottom plate to project 50mm outside the wall? which means wall just stit on the bottom plate.

much appreciated if some one clarify this.

Regards'
Magesh
 
Replies continue below

Recommended for you

The main difference between a lap welded bottom plate and a butt welded annular plate is just that, the typical weld joint. If you choose to, it is permissible to omit the annular bottom plate by butt welding the entire bottom per API 650 5.5.5.
 
If an annular plate is required, you can not use bottom plates even if the thickness is the same. They must be butt welded and annular in shape.
 
IFRs,

How to check wheather annular plate is required or not?
 
In API 650, annular plates are required in only two situations, described in sections 5.5.1 and M.4.1: the bottom ring of steel is designed using the allowable stress for materials in API Group IV or higher or if the tank is being built to Annex M and the diameter is 100 feet [30M] or more.
 