Recently while studying pipeline material(as per B31.8) I came across two material grade identification in the drawings which is tagged as L415 and 5LX60. Does anyone know what is L415? Is this a material grade similar to 5LX60? Suggest any website which gives more info on this.
 
I forgot to add that 415 in the name L415 is the minimum yield strenght for the material, 415 MPa
 
Thanks Juston, that was a great help. Much appreciated.
 