API 5L X65 is same like SA-516-65?
 
Replies continue below

Recommended for you

API-5L is a pipe spec. A516 Grade 65 is a plate spec.

Joe Tank
 
Apples and oranges: Besides product form, one's specified yield is at 65 ksi, the other's ultimate strength is at 65 ksi. They'll both rust though...

jt
 