Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API wellhead vs Process Piping 1

Status
Not open for further replies.

engr2GW

Petroleum
Nov 7, 2010
308
Hi,

I understand you can use some API materials like 4130 on process piping as long as the welding and heat treatment are done right. Can you use an ANSI and B31.3 listed materials e.g. A106B, piping and fittings in an API rated sections as long as the welding and pressure rating matches?

As much as possible, do it right the first time...
 
Replies continue below

Recommended for you

Just to clear up some misinformation.

4130 is an AISI low-alloy steel chemistry classification, not an API material. This steel can be heat treated to produce many different API pipe and tube grades. Many other API grades are made from different steels.

As to whether or not you can substitute a carbon steel pipe where a heat treated low-alloy steel pipe had been used, without knowing your application, there really is no way to be able to tell.
 