curtis2004
Mechanical
Hello all,
I am working on a small 2" drain line replacement project in NGL facility. I am using company spec to specify valves and come across with a problem. The 2" line material is 304 SST with design temperature of -100C/50C. The main reason for -100C temperature - during draining ethane can flash and cool the line. The service is sweet.
A valve vendor have 2" swing check valve ASTM A351 CF8M body, trim #10. My spec calls for ASTM A351 CF8 trim #12. 316 seems better material than 304, but how about trim? I think since this is 2" drain line and used only when the line is drained (once a 6 months) we can substitute trim #12 with trim # 10.
Do I need to check anything else before filling up request for deviation?
Thanks,
Curtis
I am working on a small 2" drain line replacement project in NGL facility. I am using company spec to specify valves and come across with a problem. The 2" line material is 304 SST with design temperature of -100C/50C. The main reason for -100C temperature - during draining ethane can flash and cool the line. The service is sweet.
A valve vendor have 2" swing check valve ASTM A351 CF8M body, trim #10. My spec calls for ASTM A351 CF8 trim #12. 316 seems better material than 304, but how about trim? I think since this is 2" drain line and used only when the line is drained (once a 6 months) we can substitute trim #12 with trim # 10.
Do I need to check anything else before filling up request for deviation?
Thanks,
Curtis