Hi Guys,
Needing your expertise on seal plush plan 11 + 61 to be used on 98wt% Sulfuric Acid Unloading Pump. Original plan is 11 + 62 which is better. However because water or steam is not allowed (not recommendable) as a quenching media because water or condensate will react with the process fluid (sulfuric acid)original plan was changed. Is this reliable?
Pump Datasheet:
Service: 98wt% Sulfuric Acid Unloading Pump
Pump Operation: Intermittent Service
Normal/Rated Capacity: 15 / 16.5 m3/hr
Pumping Temperature: 19-40 deg C
Specific Gravity @ Pumping Temperature: 1.81
Head: 29.3m
BHP Rated:4.61kw
RPM:3600
Materials:
Case/Trim class: A-8 (API Class)
Case: SS316L
Impeller: SS316L
Mechanical Seal:
Seal Flush Pipe Plan : 11+ 62 (original)
11+61 (recommendation of the pump vendor because water or steam is not allowed (not recommendable) as a quenching media because water or condensate will react with the process fluid (sulfuric acid).
Thanks in advance and more power to this site...
Needing your expertise on seal plush plan 11 + 61 to be used on 98wt% Sulfuric Acid Unloading Pump. Original plan is 11 + 62 which is better. However because water or steam is not allowed (not recommendable) as a quenching media because water or condensate will react with the process fluid (sulfuric acid)original plan was changed. Is this reliable?
Pump Datasheet:
Service: 98wt% Sulfuric Acid Unloading Pump
Pump Operation: Intermittent Service
Normal/Rated Capacity: 15 / 16.5 m3/hr
Pumping Temperature: 19-40 deg C
Specific Gravity @ Pumping Temperature: 1.81
Head: 29.3m
BHP Rated:4.61kw
RPM:3600
Materials:
Case/Trim class: A-8 (API Class)
Case: SS316L
Impeller: SS316L
Mechanical Seal:
Seal Flush Pipe Plan : 11+ 62 (original)
11+61 (recommendation of the pump vendor because water or steam is not allowed (not recommendable) as a quenching media because water or condensate will react with the process fluid (sulfuric acid).
Thanks in advance and more power to this site...