Hi all,
I have a pile 19m length with 7 shells. Each shell is 2.75m high. Diameter 8m.
In the API RP 2A, it's written:
Straightness
The maximum allowable straightness deviation in any 3 m length shall be 3 mm. For length over 3 m,
the maximum deviation of the entire length may be computed by the following formula, not to exceed
10 mm in any 12 m length.
3 mm x (total length m.)/3 m
It means that for my 1st shell it will be 3mm.
But for the 2nd shell (5.5m high) we have to calculate with the formula the total length of my pile (19m) or by section?
-1st shell 2.75m high : 3mm
-2nd shell 5.5m high : 5.5mm
-3rd shell 8.25m high : 8.25mm
-4th shell 11m high :11mm cause in any 12m length it will be 10mm.
-5th shell 13.75 high : ??? what will be the tolerance???
or
-1st shell 2.75m high : 3mm
-2nd shell 5.5m high : 19mm (formula with total length of my pile)
-3rd shell 8.25m high : 19mm(formula with total length of my pile)
-...
Many thanks if you could help me cause everybody has his own opinion on it.
Best regards
I have a pile 19m length with 7 shells. Each shell is 2.75m high. Diameter 8m.
In the API RP 2A, it's written:
Straightness
The maximum allowable straightness deviation in any 3 m length shall be 3 mm. For length over 3 m,
the maximum deviation of the entire length may be computed by the following formula, not to exceed
10 mm in any 12 m length.
3 mm x (total length m.)/3 m
It means that for my 1st shell it will be 3mm.
But for the 2nd shell (5.5m high) we have to calculate with the formula the total length of my pile (19m) or by section?
-1st shell 2.75m high : 3mm
-2nd shell 5.5m high : 5.5mm
-3rd shell 8.25m high : 8.25mm
-4th shell 11m high :
-5th shell 13.75 high : ??? what will be the tolerance???
or
-1st shell 2.75m high : 3mm
-2nd shell 5.5m high : 19mm (formula with total length of my pile)
-3rd shell 8.25m high : 19mm(formula with total length of my pile)
-...
Many thanks if you could help me cause everybody has his own opinion on it.