Hello all,
We have a vessel with Shell material of SA-387-12 CL2 and shell thickness of 105mm.This vessel needs to follow the API 934-C requirements.
API 934-C para 7.3.1 (Preheat) mandates that "All base metal should be preheat to a minimum of 300 def F during rolling.
Out vessel supplier is asking waiver to this requirement.
My question is how difficult is it to meet this requirement?
Regards,
Mechmania
We have a vessel with Shell material of SA-387-12 CL2 and shell thickness of 105mm.This vessel needs to follow the API 934-C requirements.
API 934-C para 7.3.1 (Preheat) mandates that "All base metal should be preheat to a minimum of 300 def F during rolling.
Out vessel supplier is asking waiver to this requirement.
My question is how difficult is it to meet this requirement?
Regards,
Mechmania