what exactly footnotes -a indicate , since carbon max. shown 0.45 % mass fraction for carbon however footnote-a shows 2 % mass fraction
which one is it refer max. in 0.45 or 2% mass fraction ?
 
The footnotes are intended to be informative definitions of carbon steel and low-alloy steel.

The 0.45% max shown in the table is the applicable limit for carbon and low-alloy steels.
 