Good day,
We require API 6A material(material class EE) with temperature class U (i.e. temp range -18 deg centi to + 121 deg centi) whereas vendor supplied with material having temperature class K (i.e. temp range -60 deg centi to + 82 deg centi).
Upon our comments, vendor proposed us that this material can be upgraded to class U by doing lab tests.
Can we accept this proposal? If so, then what are the lab tests required?
Note: As far as charpy test concerned, it is noted from material test certificate that test temperature is -60 deg centi and impact values are meeting API 6A requirements.
Regards
Metboss
We require API 6A material(material class EE) with temperature class U (i.e. temp range -18 deg centi to + 121 deg centi) whereas vendor supplied with material having temperature class K (i.e. temp range -60 deg centi to + 82 deg centi).
Upon our comments, vendor proposed us that this material can be upgraded to class U by doing lab tests.
Can we accept this proposal? If so, then what are the lab tests required?
Note: As far as charpy test concerned, it is noted from material test certificate that test temperature is -60 deg centi and impact values are meeting API 6A requirements.