Oct 11, 2013 #1 alby87 Materials Joined Jun 28, 2011 Messages 13 Location IT Dear All, i would ask you if it is possible to use ASTM A487-4C alloy steel at -46°C for 5000 psi .If not there is other material 60K for -46°c service? Alberto
Dear All, i would ask you if it is possible to use ASTM A487-4C alloy steel at -46°C for 5000 psi .If not there is other material 60K for -46°c service? Alberto
Oct 11, 2013 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,947 Location GB Not for PSL 3 or 4 valves. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
Not for PSL 3 or 4 valves. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer.