Hello friends
If my Procedure Qualification Report (PQR) is approved by an AI or is an AWS Standard Weld Procedure, and my internal quality assurance has a record of the Weld Procedure Qualification (WPQ) from the individual welder with a continuity record to back up continuous (usually every two month) monitoring.
is that my welder is qualified to weld on the API 650 tank by using continuity record.
i was looking in API I did not find out.
regards
Stanley
 
Replies continue below

Recommended for you

I believe API just refers to ASME for welder certification.
 
ASME IX governs welding procedure and welder qualification under API 650.
 
yes.
so my welder is qualified to weld on the API 650 tank by using continuity record.

Thanks
 