I need some information on API-650 tank designs with annular rings.
As I understand the rules, API 650 mandates an annular ring when the stress in the bottom course are above a certain level and higher strength materials are required in the shell. The Brittish standard (BS 2654) and many others mandate an annular ring when the tank is over a certain diameter (12.5m for BS 2654)
Is there anything wrong with an API-650 tank that is of large diameter (say 20-25m)that does not use the higher strength shell materials ?
Stated another way,when writing an API-650 design specification is it a good idea to mandate both the 12.5 m rule of the Brittish standard and REQUIRE an annular ring design ?
Thank you for your time
As I understand the rules, API 650 mandates an annular ring when the stress in the bottom course are above a certain level and higher strength materials are required in the shell. The Brittish standard (BS 2654) and many others mandate an annular ring when the tank is over a certain diameter (12.5m for BS 2654)
Is there anything wrong with an API-650 tank that is of large diameter (say 20-25m)that does not use the higher strength shell materials ?
Stated another way,when writing an API-650 design specification is it a good idea to mandate both the 12.5 m rule of the Brittish standard and REQUIRE an annular ring design ?
Thank you for your time