API 650, Figure 5.7a, detail b, indicates that the corner-corner weld of the flange to the neck shall be the thickness of the thinner member joined however, Figure 5.12, detail b, indicates that the corner-corner weld of the flange shall be the thickness of the thinner member joined, with a max weld of 1/2 inch.
Wouldn't the same apply to both? Is the fillet limiting note mistakenly absent from Figure 5.7a, detail b? Or, is the note mistakenly placed in Figure 5.12, detail b?