May 6, 2005 #1 emiro Mechanical Joined May 6, 2005 Messages 1 Location US Please advise us. We need to know what is the minimum distance between an annular plates joint weld and a vertical (shell) plates joint weld. Please reference the applicable API650 paragraph. Thank you in advance.
Please advise us. We need to know what is the minimum distance between an annular plates joint weld and a vertical (shell) plates joint weld. Please reference the applicable API650 paragraph. Thank you in advance.
May 17, 2005 1 #2 JoeTank Structural Joined Oct 28, 1999 Messages 1,133 Location US API-650 does not specify a minimum offset between these two joints. Steve Braune Tank Industry Consultants http://www.tankindustry.com Upvote 0 Downvote