I need to procure a sulphuric acid( Strength 98%) centrifugal pump. But the problem is that as per API 610 8th edition Table - G.1 and Table H-1, for sulphuric acid strength > 85% , the pump material class is S-1,(i.e. CS pressuer casing, CI impeller, CI inner case parts etc) and for acid consentration 85%-<1% the pump material class is A-8( AUS 316 base parts).
In short, I want to point out that for higher acid concentration pump materlals class suggested in API 610 is of lower metallurgy, while for lesser acid consentration pump material class is of higher metallurgy.
Please guide me in selecting proper Acid pump MOC.
With Regards
07071975
I need to procure a sulphuric acid( Strength 98%) centrifugal pump. But the problem is that as per API 610 8th edition Table - G.1 and Table H-1, for sulphuric acid strength > 85% , the pump material class is S-1,(i.e. CS pressuer casing, CI impeller, CI inner case parts etc) and for acid consentration 85%-<1% the pump material class is A-8( AUS 316 base parts).
In short, I want to point out that for higher acid concentration pump materlals class suggested in API 610 is of lower metallurgy, while for lesser acid consentration pump material class is of higher metallurgy.
Please guide me in selecting proper Acid pump MOC.
With Regards