Does X65 belong to a P group or is it an unspecified material?
 
Replies continue below

Recommended for you

API 5L Grade X65 is an S number 1, group 2 material. See ASME Section IX paragraph QW-420 & QW-424 for an explanation of the difference between P numbers and S numbers.
 