Jul 23, 2012 #1 Fizza453 Mechanical Joined Jun 22, 2011 Messages 262 Location AE Is there any Code Case that permits the use of API 5L X60 pipe in ASME Section VIII Division 1 construction? Nasir Welding Engineer DESCON ENGINEERING LIMITED PAKISTAN
Is there any Code Case that permits the use of API 5L X60 pipe in ASME Section VIII Division 1 construction? Nasir Welding Engineer DESCON ENGINEERING LIMITED PAKISTAN
Jul 24, 2012 #2 gr2vessels Mechanical Joined Sep 29, 2004 Messages 1,971 Location AU No, there is no Code Case allowing the use API pipe in ASME VIII-1. Cheers, gr2vessels Upvote 0 Downvote