Is there any Code Case that permits the use of API 5L X60 pipe in ASME Section VIII Division 1 construction?


Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
 
No, there is no Code Case allowing the use API pipe in ASME VIII-1.
Cheers,
gr2vessels
 