Apr 25, 2013 #1 elmio Materials Joined Feb 15, 2012 Messages 13 Location FR Dear all, I am looking for material for flange which suitable for API 5L X46 pipe class. My customer ask casted material and they sent me this: ASTM A494 F46 I have not found any F46 in this material spec. Can you recomended something? Thank you
Dear all, I am looking for material for flange which suitable for API 5L X46 pipe class. My customer ask casted material and they sent me this: ASTM A494 F46 I have not found any F46 in this material spec. Can you recomended something? Thank you
Apr 25, 2013 2 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 22,927 Location GB I think this is a typo. Try A 694. My motto: Learn something new every day Also: There's usually a good reason why everyone does it that way Upvote 0 Downvote
I think this is a typo. Try A 694. My motto: Learn something new every day Also: There's usually a good reason why everyone does it that way
Apr 26, 2013 Thread starter #3 elmio Materials Joined Feb 15, 2012 Messages 13 Location FR Thank you very much. I spent hours on it. Regrads elmio Upvote 0 Downvote
Apr 30, 2013 1 #4 hfpolo Mechanical Joined Jan 28, 2013 Messages 12 Location CO Hi. The material must be A694 F46. greetings to all. Upvote 0 Downvote
Apr 30, 2013 Thread starter #5 elmio Materials Joined Feb 15, 2012 Messages 13 Location FR Thank you hfpolo! It was a typing error by customer. Our sales team did enough mistake that case I did not want ask back to the customer. Regards Elmio Upvote 0 Downvote
Thank you hfpolo! It was a typing error by customer. Our sales team did enough mistake that case I did not want ask back to the customer. Regards Elmio